| Product Description | ||||
|
This grade is characterized by excellent gloss and good surface hardness. Typical applications are sanitary, closures with and without integral hinges.
The product mentioned herein is in particular not tested and therefore not validated for use in pharmaceutical/medical applications. |
||||
| General | ||||
|
Material Status
|
|
|||
|
Availability
|
|
|||
|
Features
|
|
|||
|
Uses
|
|
|||
|
UL File Number
|
|
|||
|
Forms
|
|
|||
|
Processing Method
|
|
|||
| Physical |
Nominal Value
|
Unit
|
Test Method
|
|
Density
|
|
g/cm³
|
ISO 1183 |
|
Melt Mass-Flow Rate (MFR)
|
ISO 1133 | ||
|
230°C/2.16 kg
|
|
g/10 min
|
|
|
230°C/5.0 kg
|
|
g/10 min
|
|
| Mechanical |
Nominal Value
|
Unit
|
Test Method
|
|
Tensile Stress
|
ISO 527-2 | ||
|
Yield
|
|
psi
|
|
|
Break
|
|
psi
|
|
|
Tensile Strain (Break)
|
|
%
|
ISO 527-2 |
|
Flexural Modulus
|
|
psi
|
ASTM D790 |
| Impact |
Nominal Value
|
Unit
|
Test Method
|
|
Charpy Notched Impact Strength (73°F)
|
|
ft·lb/in²
|
ISO 179 |
|
Notched Izod Impact Strength (73°F)
|
|
ft·lb/in²
|
ISO 180/4A |
| Hardness |
Nominal Value
|
Unit
|
Test Method
|
|
Shore Hardness (Shore D)
|
|
|
ISO 868 |
| Thermal |
Nominal Value
|
Unit
|
Test Method
|
|
Heat Deflection Temperature
|
|||
|
66 psi, Unannealed
|
|
°F
|
ISO 75-2/B |
|
264 psi, Unannealed
|
|
°F
|
ISO 75-2/A |
|
Vicat Softening Temperature
|
|||
|
--
|
|
°F
|
ISO 306/A |
|
--
|
|
°F
|
ISO 306/B |
| Related Terminology | |||
|
Product names can be difficult to match. You may have searched any one of these terms to find this product: SABIC® PP 571P, SABIC PP 571P, SABIC® PP , SABIC PP, SABICPP571P, SABICPP, PP 571 P, PP571P, PP571, PP, 571 P, 571P, Polypropylene Homopolymer, PP Homopolymer, Polypropylene, SABIC, PolypropyleneHomopolymer, PPHomopolymer, P571, 571PP
|
|||
| Features | |||
|
Features may also be described by the following terms: High Gloss.
|
|||
| Notes |
| 1Typical properties: these are not to be construed as specifications. |