Polycarbonate (PC): TES

Produto Disponibilidade Descrição do produto
TES J-50/10 BK223 África & Oriente Médio  
TES J-50/10 GY8440 África & Oriente Médio  
TES J-50/10 África & Oriente Médio
Molding Parameters: 4 hours recommended for high tensile strength and smooth surface finish, or for vacuum metalizing. The dry temperature at 16 hours is 180°F. For 2-zone machines, the rear temperature is 600-650°F, and the front temperature is 580-620°F.
TES J-50/20 BK223 África & Oriente Médio  
TES J-50/20 GY8134 África & Oriente Médio  
TES J-50/20 NAT África & Oriente Médio  
TES J-50/20/FR BK3585 África & Oriente Médio  
TES J-50/20/FR NAT África & Oriente Médio  
TES J-50/20/RG BK223 África & Oriente Médio  
TES J-50/20/RG RD8664 África & Oriente Médio
09447
TES J-50/20/RG África & Oriente Médio
Molding Parameters: 4 hours recommended for high tensile strength and smooth surface finish, or for vacuum metalizing. The dry temperature at 16 hours is 180°F. For 2-zone machines, the rear temperature is 600-650°F, and the front temperature is 580-620°F.
TES J-50/20/TF/10 BK África & Oriente Médio  
TES J-50/20 África & Oriente Médio  
TES J-50/30 BK223 África & Oriente Médio  
TES J-50/30 NAT África & Oriente Médio  
TES J-50/30/FR BK3585 África & Oriente Médio  
TES J-50/30/RG BK223 África & Oriente Médio  
TES J-50/30/RG África & Oriente Médio
Molding Parameters: 4 hours recommended for high tensile strength and smooth surface finish, or for vacuum metalizing. The dry temperature at 16 hours is 180°F. For 2-zone machines, the rear temperature is 600-650°F, and the front temperature is 580-620°F.
TES J-50/30/TF/15 BK3585 África & Oriente Médio  
TES J-50/30/TF/15 GY8436 África & Oriente Médio  
TES J-50/30/TF/15 NAT África & Oriente Médio  
TES J-50/30 África & Oriente Médio
Molding Parameters: 4 hours recommended for high tensile strength and smooth surface finish, or for vacuum metalizing. The dry temperature at 16 hours is 180°F. For 2-zone machines, the rear temperature is 600-650°F, and the front temperature is 580-620°F.
TES J-50/40 BK223 África & Oriente Médio  
TES J-50/40 WT8193 África & Oriente Médio  
TES J-50/40/ NAT África & Oriente Médio  
TES J-50/40 África & Oriente Médio
Molding Parameters: 4 hours recommended for high tensile strength and smooth surface finish, or for vacuum metalizing. The dry temperature at 16 hours is 180°F. For 2-zone machines, the rear temperature is 600-650°F, and the front temperature is 580-620°F.