Polykarbonat (PC): TES
Produkt | Verfügbarkeit | Produktbeschreibung |
---|---|---|
TES J-50/10 BK223 | Afrika und Mittlerer Osten | |
TES J-50/10 GY8440 | Afrika und Mittlerer Osten | |
TES J-50/10 | Afrika und Mittlerer Osten |
Molding Parameters:
4 hours recommended for high tensile strength and smooth surface finish, or for vacuum metalizing.
The dry temperature at 16 hours is 180°F.
For 2-zone machines, the rear temperature is 600-650°F, and the front temperature is 580-620°F.
|
TES J-50/20 BK223 | Afrika und Mittlerer Osten | |
TES J-50/20 GY8134 | Afrika und Mittlerer Osten | |
TES J-50/20 NAT | Afrika und Mittlerer Osten | |
TES J-50/20/FR BK3585 | Afrika und Mittlerer Osten | |
TES J-50/20/FR NAT | Afrika und Mittlerer Osten | |
TES J-50/20/RG BK223 | Afrika und Mittlerer Osten | |
TES J-50/20/RG RD8664 | Afrika und Mittlerer Osten |
09447
|
TES J-50/20/RG | Afrika und Mittlerer Osten |
Molding Parameters:
4 hours recommended for high tensile strength and smooth surface finish, or for vacuum metalizing.
The dry temperature at 16 hours is 180°F.
For 2-zone machines, the rear temperature is 600-650°F, and the front temperature is 580-620°F.
|
TES J-50/20/TF/10 BK | Afrika und Mittlerer Osten | |
TES J-50/20 | Afrika und Mittlerer Osten | |
TES J-50/30 BK223 | Afrika und Mittlerer Osten | |
TES J-50/30 NAT | Afrika und Mittlerer Osten | |
TES J-50/30/FR BK3585 | Afrika und Mittlerer Osten | |
TES J-50/30/RG BK223 | Afrika und Mittlerer Osten | |
TES J-50/30/RG | Afrika und Mittlerer Osten |
Molding Parameters:
4 hours recommended for high tensile strength and smooth surface finish, or for vacuum metalizing.
The dry temperature at 16 hours is 180°F.
For 2-zone machines, the rear temperature is 600-650°F, and the front temperature is 580-620°F.
|
TES J-50/30/TF/15 BK3585 | Afrika und Mittlerer Osten | |
TES J-50/30/TF/15 GY8436 | Afrika und Mittlerer Osten | |
TES J-50/30/TF/15 NAT | Afrika und Mittlerer Osten | |
TES J-50/30 | Afrika und Mittlerer Osten |
Molding Parameters:
4 hours recommended for high tensile strength and smooth surface finish, or for vacuum metalizing.
The dry temperature at 16 hours is 180°F.
For 2-zone machines, the rear temperature is 600-650°F, and the front temperature is 580-620°F.
|
TES J-50/40 BK223 | Afrika und Mittlerer Osten | |
TES J-50/40 WT8193 | Afrika und Mittlerer Osten | |
TES J-50/40/ NAT | Afrika und Mittlerer Osten | |
TES J-50/40 | Afrika und Mittlerer Osten |
Molding Parameters:
4 hours recommended for high tensile strength and smooth surface finish, or for vacuum metalizing.
The dry temperature at 16 hours is 180°F.
For 2-zone machines, the rear temperature is 600-650°F, and the front temperature is 580-620°F.
|