Home > Plastics > Materials > NORYL™ > NORYL™ WCA105 resin - Datasheet

NORYL™ WCA105 resin Data Sheet

Polyphenylene Ether + TPE

Supplied by SABIC Innovative Plastics

View Complete Data Sheet Search 96000+ Data Sheets
Create Your Free Account!
Product Description
NORYL™ 
WCA105 resin
Flexible, non-halogenated FR mPPE extrusion grade ideal for evaluation in applications such as wire insulation. Flame retardant performance capable of meeting VW1 and 105C temperature rating requirements as defined by UL 1581. 56 Shore D hardness. Excellent processing using standard extrusion equipment. UL 1581 tests conducted on 2.0 mm wire with 0.12 mm x 20 stranded copper conductor.
NORYL™ 
WCA105 resin
Flexible, non-halogenated FR mPPE extrusion grade ideal for evaluation in applications such as wire insulation. Flame retardant performance capable of meeting VW1 and 105C temperature rating requirements as defined by UL 1581. 56 Shore D hardness. Excellent processing using standard extrusion equipment. UL 1581 tests conducted on 2.0 mm wire with 0.12 mm x 20 stranded copper conductor.
NORYL™ 
WCA105 resin
Flexible, non-halogenated FR mPPE extrusion grade ideal for evaluation in applications such as wire insulation. Flame retardant performance capable of meeting VW1 and 105C temperature rating requirements as defined by UL 1581. 56 Shore D hardness. Excellent processing using standard extrusion equipment. UL 1581 tests conducted on 2.0 mm wire with 0.12 mm x 20 stranded copper conductor.
General NORYL™ 
WCA105 resin
NORYL™ 
WCA105 resin
NORYL™ 
WCA105 resin
Material Status 
  • Commercial: Active
  • Commercial: Active
  • Commercial: Active
Availability 
  • North America
  • Asia Pacific
  • Europe
Additive 
  • Flame Retardant
  • Flame Retardant
  • Flame Retardant
Features 
  • Flame Retardant
  • Good Flexibility
  • Good Processability
  • Halogen Free
  • Flame Retardant
  • Good Flexibility
  • Good Processability
  • Halogen Free
  • Flame Retardant
  • Good Flexibility
  • Good Processability
  • Halogen Free
Uses 
  • Insulation
  • Wire & Cable Applications
  • Insulation
  • Wire & Cable Applications
  • Insulation
  • Wire & Cable Applications
Agency Ratings 
RoHS Compliance 
--
--
Processing Method 
  • Extrusion Coating
  • Extrusion Coating
  • Extrusion Coating
Physical NORYL™ 
WCA105 resin
NORYL™ 
WCA105 resin
NORYL™ 
WCA105 resin
Unit
Test Method
Specific Gravity
 
ASTM D792
Melt Mass-Flow Rate (MFR) (250°C/10.0 kg)
g/10 min
ASTM D1238
Water Absorption 2 (73°F, 24 hr)
%
ASTM D570
Mechanical NORYL™ 
WCA105 resin
NORYL™ 
WCA105 resin
NORYL™ 
WCA105 resin
Unit
Test Method
Tensile Strength
         
Break
psi
UL 1581
Break 3
psi
ASTM D638
Break, 277°F 4
psi
UL 1581
Break
psi
ISO 527-2/50
Tensile Elongation
         
Break
%
UL 1581
Break 3
%
ASTM D638
Break, 277°F 4
%
UL 1581
Break
%
ISO 527-2/50
Flexural Modulus 5
         
3.94 in Span
psi
ASTM D790
--
psi
ISO 178
Films NORYL™ 
WCA105 resin
NORYL™ 
WCA105 resin
NORYL™ 
WCA105 resin
Unit
Test Method
Trouser Tear Resistance
lbf/in
ISO 6383-1
Hardness NORYL™ 
WCA105 resin
NORYL™ 
WCA105 resin
NORYL™ 
WCA105 resin
Unit
Test Method
Shore Hardness (Shore D)
 
ISO 868
Thermal NORYL™ 
WCA105 resin
NORYL™ 
WCA105 resin
NORYL™ 
WCA105 resin
Unit
Test Method
Deflection Temperature Under Load (66 psi, Unannealed, 0.252 in)
°F
ASTM D648
Brittleness Temperature
°F
ASTM D746
Vicat Softening Temperature
°F
ISO 306/A50
UL Temperature Rating
°F
UL 1581
Heat Deformation 6 (250°F)
%
UL 1581
Electrical NORYL™ 
WCA105 resin
NORYL™ 
WCA105 resin
NORYL™ 
WCA105 resin
Unit
Test Method
Volume Resistivity
ohm·cm
IEC 60093
Electric Strength (0.0787 in, in Oil)
V/mil
IEC 60243-1
Relative Permittivity
        IEC 60250
50 Hz
 
 
60 Hz
 
 
1 MHz
 
 
Dissipation Factor
        IEC 60250
50 Hz
 
 
60 Hz
 
 
1 MHz
 
 
Comparative Tracking Index
V
IEC 60112
Flammability NORYL™ 
WCA105 resin
NORYL™ 
WCA105 resin
NORYL™ 
WCA105 resin
Unit
Test Method
Glow Wire Flammability Index (0.118 in)
°F
IEC 60695-2-12
Glow Wire Ignition Temperature (0.118 in)
°F
IEC 60695-2-13
Oxygen Index
%
ISO 4589-2
Smoke Density
        ASTM E662
Flame, 0.5 mm plaque, Ds, max
 
 
Non-Flame, 0.5 mm plaque, Ds, max
 
 
VW-1
 
UL 1581
Related Terminology
NORYL™ 
WCA105 resin
This supplier and product may also be known by these terms: GE Plastics, LNP Engineering Plastics, GE Polymerland
NORYL™ 
WCA105 resin
This supplier and product may also be known by these terms: GE Plastics, LNP Engineering Plastics
NORYL™ 
WCA105 resin
This supplier and product may also be known by these terms: GE Plastics Europe, LNP Engineering Plastics, GE Polymerland Europe, GE Polymerland, GE Plastics
Features
NORYL™ 
WCA105 resin
Features may also be described by the following terms: Good Processability, Easy Processing, Zero Halogen Content, Halogen Free, Good Flexibility, Flexible.
NORYL™ 
WCA105 resin
Features may also be described by the following terms: Good Flexibility, Flexible, Good Processability, Easy Processing, Zero Halogen Content, Halogen Free.
NORYL™ 
WCA105 resin
Features may also be described by the following terms: Good Processability, Easy Processing, Good Flexibility, Flexible, Zero Halogen Content, Halogen Free.
Uses
NORYL™ 
WCA105 resin
Uses may also be described by the following terms: Wire and Cable Applications, Wire & Cable Applications.
NORYL™ 
WCA105 resin
Uses may also be described by the following terms: Wire and Cable Applications, Wire & Cable Applications.
NORYL™ 
WCA105 resin
Uses may also be described by the following terms: Wire and Cable Applications, Wire & Cable Applications.
Agency Ratings
NORYL™ 
WCA105 resin
This plastic material has 2 certifications from the following agencies (the number in parentheses shows the number of certifications for that agency): UL (2).
NORYL™ 
WCA105 resin
This plastic material has 2 certifications from the following agencies (the number in parentheses shows the number of certifications for that agency): UL (2).
NORYL™ 
WCA105 resin
This plastic material has 2 certifications from the following agencies (the number in parentheses shows the number of certifications for that agency): UL (2).
Available Documents
NORYL™ 
WCA105 resin
Technical Datasheet
NORYL™ 
WCA105 resin
Technical Datasheet
NORYL™ 
WCA105 resin
Technical Datasheet
Extrusion NORYL™ 
WCA105 resin
NORYL™ 
WCA105 resin
NORYL™ 
WCA105 resin
Unit
 
Drying Temperature
°F
 
Drying Time
hr
 
Suggested Max Moisture
%
 
Cylinder Zone 1 Temp.
°F
 
Cylinder Zone 3 Temp.
°F
 
Cylinder Zone 5 Temp.
°F
 
Melt Temperature
°F
 
Die Temperature
°F
 
Extrusion Notes
NORYL™ 
WCA105 resin
Conductor Pre-heat Temperature: 80 - 150 °C
Cooling Water Air Gap: 100 - 200 mm
Cross-head Temperature: 250 - 285 °C
Drying Time (Cumulative): 12 hrs
Extruder Length/Diameter Ratio (L/D): 22:1 to 26:1
Neck Temperature: 250 - 285 °C
Screen Pack: 150 - 100
Screw Speed: 15 - 40 rpm
Water Bath Temperature: 15 - 80 °C
NORYL™ 
WCA105 resin
Conductor Pre-heat Temperature: 80 - 150 °C
Cooling Water Air Gap: 100 - 200 mm
Cross-head Temperature: 250 - 285 °C
Drying Time (Cumulative): 12 hrs
Extruder Length/Diameter Ratio (L/D): 22:1 to 26:1
Neck Temperature: 250 - 285 °C
Screen Pack: 150 - 100
Screw Speed: 15 - 40 rpm
Water Bath Temperature: 15 - 80 °C
NORYL™ 
WCA105 resin
Conductor Pre-heat Temperature: 80 - 150 °C
Cooling Water Air Gap: 100 - 200 mm
Cross-head Temperature: 250 - 285 °C
Drying Time (Cumulative): 12 hrs
Extruder Length/Diameter Ratio (L/D): 22:1 to 26:1
Neck Temperature: 250 - 285 °C
Screen Pack: 150 - 100
Screw Speed: 15 - 40 rpm
Water Bath Temperature: 15 - 80 °C
Notes
1Typical properties: these are not to be construed as specifications.
2Results measured at 48 hrs
3Type I, 2.0 in/min
4After 7 days
50.49 in/min
6250 g
 
UL and the UL logo are trademarks of UL LLC © 2014. All Rights Reserved.
The information presented on this datasheet was acquired by UL Prospector from the producer of the material. UL Prospector makes substantial efforts to assure the accuracy of this data. However, UL Prospector assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.